Item | Index |
Type | Addition-type liquid silicone |
Shore Hardness | 33 Shore A |
Kinematic Viscosity | 300000 cP (centipoise) |
Elongation at Break | ≥462% |
Tensile Strength | ≥1015.3 psi |
Tear Strength | ≥4.3 MPa |
Solid Content | ≥98% |
Specific Gravity (25℃) | 0.95 |
Pot Life | 72 h |
Shelf Life (Unopened) | 360 days |
Flash Drying Temperature | 100-120℃ |
Final Drying Temperature | 120℃ |
This data is not for specification formulation. Our company has a variety of liquid silicone products with different technical parameters. Please contact the nearest sales office of Zhumao New Materials to select the suitable product model before formulating specifications. | |
Common Problems and Solutions | ||
Common Problems | Causes | Solutions |
Silicone not curing/sticky surface | 1. Deviated catalyst ratio with inaccurate measurement 2. Substrate fading, chemical reaction between colorant and silicone platinum water 3. Use of non-special diluent/additives 4. No additional catalyst added after adding color paste/brightener | 1. Use an electronic scale to accurately prepare the catalyst ratio 2. Conduct color fixing treatment in advance for fading-prone substrates 3. Use only the special supporting additives for this product 4. Add catalyst in the same proportion after adding color paste/brightener |
Bubbles in the formed film | 1. Excessively high flash/final drying temperature, rapid baking 2. No standing and defoaming after silicone stirring, surface drying too fast wrapping bubbles | 1. Lower the baking temperature, extend the baking time and avoid rapid baking 2. Let the mixture stand for 10-15min to defoam after preparation, and use slow-drying catalyst to slow down the surface drying speed |
Silicone penetrating the substrate | Low silicone viscosity with insufficient compatibility | Replace with a special base paste with higher viscosity, or increase the number of base coat printing layers |
Poor adhesion, easy to fall off | 1. Unclean substrate surface 2. Mismatch between addition-type silicone and fabric groups | 1. Re-clean the substrate surface 2. Use a special primer for the corresponding fabric to improve interlayer adhesion |